MRD evaluated MRO Gen II in a natural-rubber/polybutadiene off-the-road tread using a semi-efficient vulcanization cure system and standard rubber-processing methods.
Tensile properties remained broadly stable, while peak tear strength and tear toughness improved. Cut-and-chip volume loss also decreased without a negative effect on dynamic properties.
A dynamic-mechanical rolling-resistance indicator measured at 10% strain, 10 Hz and 60°C showed slight improvement after the formulation was optimized for MRO Gen II.
The results indicate a path to longer-lived severe-service tires that maintain expected fuel-economy performance.